Why TGA Residue Is Not Filler Percentage in Plastics

Estimated read time 5 min read

Understanding What Thermogravimetric Analysis Actually Measures

Thermogravimetric analysis, commonly abbreviated as TGA, is a widely used technique for studying how a material loses mass as it is heated under controlled conditions. In the context of packaging plastics, TGA is often used to estimate the amount of filler, pigment, or inorganic additive present in a compound. A common assumption is that the mass remaining after the polymer has decomposed — the "residue" — directly equals the percentage of a single, specific filler. This assumption is a frequent source of confusion, and it is worth unpacking why it is not automatically true.

What TGA Residue Actually Represents

TGA works by heating a small sample in a controlled atmosphere, typically nitrogen or air, while continuously recording its mass. As temperature rises, organic components such as the base polymer, processing additives, and certain coatings volatilize or decompose, releasing gases and reducing the sample's mass. What remains at the end of the heating program — the residue — is simply whatever did not decompose or volatilize under those specific conditions. This residue is a mass fraction, not a chemical identification. TGA tells you how much mass is left; it does not tell you what that mass is made of.

A Hypothetical Example: A Compact Powder Case Compound

Consider a purely hypothetical scenario to illustrate the point. Imagine a compact powder case molded from a polymer blend that contains three distinct non-volatile components: a mineral filler used for stiffness, a small amount of carbon black used for color and UV stabilization, and trace metallic residue from a pigment masterbatch. If this hypothetical sample is subjected to TGA and shows a 12 percent residue at the end of the test, it would be incorrect to conclude that the mineral filler alone makes up 12 percent of the formulation. In this hypothetical case, the 12 percent figure could represent the mineral filler, the carbon black, the pigment residue, and any inorganic contamination, all combined. Without additional analysis, there is no way to separate these contributions from the TGA curve alone.

Why a Single Number Cannot Isolate One Filler

Several real technical factors explain why TGA residue is not automatically attributable to one filler:

Overlapping decomposition behavior. Many organic additives, carbon black, and certain polymer chars do not fully combust or volatilize at the temperatures used in a standard TGA run, especially under an inert atmosphere. This means that material other than the intended inorganic filler can remain in the residue, inflating the apparent filler content.

Atmosphere dependence. The same hypothetical sample can produce different residue values depending on whether the test is run in nitrogen or air. Carbon black, for example, typically does not oxidize away under nitrogen but will largely burn off under air at sufficiently high temperature. If the atmosphere and temperature program are not matched to the specific components in the formulation, the residue value can be misleading.

Multiple fillers or additives in one formulation. Packaging plastics frequently contain more than one non-volatile ingredient — for example, a combination of mineral fillers, flame-retardant residues, and pigment carriers. TGA reports only the combined mass of everything that survives the heating program. It cannot, by itself, distinguish a calcium carbonate filler from a titanium dioxide pigment or from residual catalyst ash.

Sample heterogeneity. A TGA test typically uses a very small sample mass, often just a few milligrams. If the filler is not perfectly homogeneous throughout the part — which can happen in thicker-walled packaging components — the small sample may not be representative of the bulk material, and the measured residue may not reflect the true average filler loading.

Baseline and calibration effects. Instrument calibration, pan material, heating rate, and even moisture content in the sample can shift the apparent residue by small amounts. These effects are generally minor but can matter when precise quantification is the goal.

Why Complementary Methods Matter

Because TGA residue is a mass-based measurement rather than a compositional one, it is generally paired with other analytical techniques when precise filler identification is required. Techniques such as X-ray fluorescence, elemental analysis, or ash composition studies are typically used alongside TGA to determine what elements or compounds make up the residue. Microscopy and spectroscopic methods can further help confirm whether a residue is dominated by a mineral filler, a pigment, or trace contamination. In short, TGA answers "how much mass is left," while complementary methods are needed to answer "what that mass actually is."

Method Limitations to Keep in Mind

It is also worth stating the limitations of TGA plainly. TGA does not identify molecular structure, does not distinguish between chemically similar inorganic compounds, and is sensitive to test parameters such as heating rate, gas flow, and sample pan geometry. Results from one laboratory setup are not always directly comparable to another unless the test conditions are closely matched. For packaging plastics specifically, where formulations often combine recycled content, pigments, and functional fillers, these limitations mean that a single residue percentage should be interpreted cautiously rather than treated as a definitive filler content figure.

Material Complexity in Packaging Plastics

A2dad28f8bdd5be5b2b4a795e14b7e66

Packaging sample showroom of SamBound New Material Technology Company Ltd. (sambound.com).

 

This complexity is one reason why material selection for cosmetic packaging — such as choosing between AS and PMMA resins, or evaluating PCR-content PET versus virgin material — requires more than a single data point. Understanding how a given formulation behaves across multiple test methods, not just one TGA run, is part of sound material science practice in packaging development.

A Note on Visual Material

Where Manufacturing Expertise Fits In

Conclusion